Some common problems in the firing of zirconia ceramics
Jul 29, 2021
The ceramic green body is composed of many individual solid particles before sintering. There are a large number of pores in the green body. The porosity is generally 35%~60% (that is, the relative density of the green body is 40%~65%). The value depends on the characteristics of the powder itself and the molding method and technology used. When the solid billet is heated at high temperature, the particles in the billet will migrate. After reaching a certain temperature, the billet will shrink, and crystal grains will grow. With the elimination of pores, it will eventually be at a temperature below the melting point (usually at a temperature below the melting point). 0.5 to 0.7 times the melting point) the green body becomes a dense polycrystalline ceramic material. This process is called sintering.
Sintering is a process after the ceramic body is formed. A large part of the performance of ceramic products is determined by sintering. Zirconia ceramics must be sintered with high density and uniformity. Not only is the degreasing step of the previous processing procedure essential, but also affected by factors such as powder, additives, sintering temperature and time, pressure and sintering atmosphere.
In the specific sintering process, the zirconia ceramic body may have problems such as deformation, cracking, abnormal growth of crystal grains, etc. What are the possible reasons? Let's analyze the specific problems in detail below.
1. Deformation:
The zirconia ceramics deform during the sintering process. The reason may be that the powder particle size distribution is too wide; the selection and amount of additives in the powder are unreasonable; the shrinkage of the ceramic is inconsistent.
The inconsistent shrinkage of ceramics is due to the following three reasons:
① The furnace temperature is not uniform, and the ceramic body shrinks inconsistently;
② The heating speed is fast, and the temperature conduction produces a gradient. The closer the ceramic body is to the surface, the faster it shrinks, and the closer it is to the center, the slower it shrinks.
③ There is a density gradient. During molding, due to factors such as pressure and filler, the internal shrinkage ratio of the blank is inconsistent.
2: Rupture
The main reason for the cracking of the sintered ceramic body is that there are defects in the ceramic body, and it is also related to the shrinkage of the green body. The reason for the inconsistent shrinkage of the green body is referred to the analysis of the reasons for sintering deformation.
When the shrinkage is inconsistent, if there are defects (holes, dark cracks, etc.), the defects become the source of fracture, and the crack propagation causes the green body to crack.
3. The crystal grain grows abnormally
When the grains grow abnormally, there are often a large number of pores in these excessively large grains, which are difficult to be discharged from the grains to the grain boundaries, which will make it difficult for the ceramic material to achieve higher density and many properties of the material. Deterioration, especially mechanical properties (fracture toughness, flexural strength, etc.).
The main reasons for the abnormal growth of crystal grains are as follows:
① The particle size distribution range of the original powder is too wide, that is, the large particles in the powder are larger or much larger than 2 times the average grain size;
② The density of the green body is uneven during molding (powder agglomeration, the pressing pressure of the green body has a gradient, and the additive is uneven), and uneven densification occurs in the sintering;
③ Too high sintering temperature and too long holding time.